1-20 of 79 Search Results for

Babbitt

Follow your search
Access your saved searches in your account

Would you like to receive an alert when new items match your search?
Close Modal
Sort by
Journal Articles
SPE J. 7 (04): 342–346.
Paper Number: SPE-1682-PA
Published: 01 December 1967
...Richard W. Hanks The method of Caldwell and Babbitt for determining Bingham plastic rheological constants from engineering pipe flow data has been erroneously used in many previous applications. A reanalysis of extensive pipe flow data from the literature is performed. Critical Reynolds numbers...
Proceedings Papers

Paper presented at the SPE Annual Technical Conference and Exhibition, October 8–10, 2012
Paper Number: SPE-159346-MS
Proceedings Papers

Paper presented at the SNAME 11th Propeller and Shafting Symposium, September 12–13, 2006
Paper Number: SNAME-PSS-2006-18
... PTFE faced bearing technology, already established for hydro generator use, has been further developed for civil and military marine applications. The paper describes this type of bearing and the advantages compared with conventional babbitt. Details of testing and a description of a PTFE-faced...
Journal Articles
J Pet Technol 23 (09): 1081–1088.
Paper Number: SPE-3215-PA
Published: 01 September 1971
... were compared so that additional scale-model values could be predicted. Introduction Several noteworthy publications written before 1960 apply either directly or indirectly to the problems in fluid flow with which we are concerned here. Among them are the Babbitt and Caldwell report of experiments...
Proceedings Papers

Paper presented at the Middle East Technical Conference and Exhibition, February 25–28, 1979
Paper Number: SPE-7860-MS
.... Satisfactory operation in this case means providing the required power under all site conditions utile burning either NGL or crude. Midstream Oil & Gas maintenance piping simulation east-west petrotine operation piping design prime mover pipeline babbitt bearing gas turbine reliability...
Proceedings Papers

Paper presented at the Abu Dhabi International Petroleum Exhibition & Conference, November 11–14, 2019
Paper Number: SPE-197591-MS
.... Sour Gas Failures of Hydrodynamic Journal bearings Sour gas can affect the performance of hydrodynamic bearings. White metal babbitt materials high in copper content are prone to corrosion by hydrogen sulfide and carbonyl sulfide. An example of a failed hydrodynamic journal is shown in Figure 6...
Images
SEM-EDS surface analysis of white metal bearing surface submersed in uninhi...
Published: 11 November 2019
Figure 15 SEM-EDS surface analysis of white metal bearing surface submersed in uninhibited control oil, exposed to 2000 PPM hydrogen sulfide gas in methane; 120°C, 24 BAR 30 days. Copper sulfide "bloom" has formed on surface of babbitt metal. More
Images
SEM-EDS surface analysis of white metal bearing surface submersed in CPI in...
Published: 11 November 2019
Figure 16 SEM-EDS surface analysis of white metal bearing surface submersed in CPI inhibited test lubricant, exposed to 2000 PPM hydrogen sulfide gas in methane; 120oC, 24 BAR 30 days. No copper sulfide "bloom" has formed on surface of babbitt metal. More
Journal Articles
J Ship Prod Des 3 (04): 256–263.
Paper Number: SNAME-JSP-1987-3-4-256
Published: 01 November 1987
..., labyrinth seals, packing sleeves and babbitt bearings. The need for thermal spray repair is evident during ship overhauls, when critical time and cost schedules must be met. The applications listed are under evaluation in the test pro- grams to establish confidence in thermal spraying. New can- didates...
Journal Articles
Trans. G-25 (01): 179–182.
Paper Number: SPE-925179-G
Published: 01 December 1925
..., a gasket of mixed lead and babbitt was poured into the packing recess of the clamp, using the duplicate 12in. collar as a form to mold in the babbitt a groove corresponding as nearly as possible to the irregularities of the 12Yz-in. landing collar. The clamp was then replaced between the lO-in. and 12in...
Proceedings Papers

Paper presented at the SPE/IATMI Asia Pacific Oil & Gas Conference and Exhibition, October 17–19, 2017
Paper Number: SPE-186882-MS
... characteristic for a specific material at a specific temperature. This particular condition despite there no applied cyclic loading through bearing service condition, fatigue failure was initiated due to un-equilibrium loading condition and the low strength of the Babbitt. Tin base Babbitt's commonly contain...
Journal Articles
SPE Prod & Oper 35 (01): 001–008.
Paper Number: SPE-190939-PA
Published: 17 February 2020
... brine and Pb. Babbitt metals are used to coat the surface of the thrust‐bearing pads. The name, which refers to several Pb‐ or tin‐based alloys, was taken from its initial creator Isaac Babbitt when he first formulated the alloy in 1839 with a composition of 89.3 wt% tin, 7.1 wt% antimony, and 3.6...
Journal Articles
Trans. 82 (01): 75–89.
Paper Number: SPE-929075-G
Published: 01 December 1929
... equipped with 12-ft. wheels. The latter reduce the belt tension required, and provide a greater radius for bandwheel type counterbalances. Rig irons are of nominaI6-in. size. Many of the old-fashioned wooden pitmans with babbitt and wooden block bearings are still in use, but are being gradually superseded...
Proceedings Papers

Paper presented at the SNAME 7th International Symposium on Ship Operations, Management and Economics, April 6–7, 2021
Paper Number: SNAME-SOME-2021-003
... by a gravity tank which is fitted higher than the highest waterline. Bearings are made of a cast iron bush, lined with white metal also known as babbitt. Tin-based or lead-based babbitt is the most popular bearing material. It combines strength, tolerance to dirt, low coefficient of friction and low...
Journal Articles
J Pet Technol 3 (06): 159–164.
Paper Number: SPE-951159-G
Published: 01 June 1951
... presented at the Petroleum Branch Fall Meeting in New Orleans. La . Oct. 4-6. 1950. been a subject of interest. Beck, Nuss, and Dunn: following Caldwell and Babbitt: base their calculations for non-turbu- lent flow on Buckingham's integration of Bingham's law for pipe flow and measurements of the plastic...
Journal Articles
J Can Pet Technol 37 (05).
Paper Number: PETSOC-98-05-01
Published: 01 May 1998
... to the effect of freezing on dewater- ability of drilling muds. The dewaterability enhancement caused by freezing has been long known. In 1919, Babbitt and Schlenz demonstrated the benefit of freezing wastewater sludge( 9 ). They noted that after the sludge was frozen on a sand drying bed during the winter...
Journal Articles
SPE Prod & Oper 1 (04): 279–288.
Paper Number: SPE-14584-PA
Published: 01 July 1986
... the thrust-bearing load-carrying capability, the steel tilting bearing pads were exchanged for copper bearing pads. Both pad designs have a very thin babbitt layer at the sliding face. Copper has the outstanding advantage because of its higher thermal conductivity (more than eight times that of steel...
Journal Articles
SPE Res Eval & Eng 23 (03): 1045–1059.
Paper Number: SPE-195282-PA
Published: 13 August 2020
... Location of J‐557 injector in Ranger Fault Block 6 and schematic of perforated intervals. The bottomhole pressure was recorded directly with a downhole gauge and calculated from surface pressure using a tubing friction allowance as seen in Eq. 3 (Babbitt and Doland 1949 ; Turneaure and Russell...
Proceedings Papers

Paper presented at the SNAME 8th Propeller and Shafting Symposium, September 23–24, 1997
Paper Number: SNAME-PSS-1997-09
... in a vertical boring miJI and the upper end offset in such a manner that only the bottom half of the babbitt is machined, starting with .004" and tapering off to zero, 20 inches in. The net result on the bearing is similar to what could be accomplished by the prolonged method of bluing and scraping the bottom...

Product(s) added to cart