Paper presented at the CORROSION 2011, March 13–17, 2011
Paper Number: NACE-11409
... ABSTRACT: The hot corrosion resistance of nickel- base superalloys ChS91VI and EP708 for stator parts of marine gas turbine engines is investigated. The resistance to hot corrosion of superalloys ChS91VI and EP708 at 700oC are determined mainly by the microstructure of grain boundaries...